MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Axiall 9202J Rigid PVC, Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 9202J is suitable for all types of food packaging. The compound provides low taste and odor properties and contains an ultraviolet light stabilizer which protects light sensitive products.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 41.4 MPa6000 psiASTM D-638
Tensile Modulus 2.41 GPa350 ksiASTM D-638
Flexural Strength 69.6 MPa10100 psiASTM D-790
Flexural Modulus 2.24 GPa325 ksiASTM D-790
Izod Impact, Notched  7.47 J/cm
@Thickness 6.35 mm
14.0 ft-lb/in
@Thickness 0.250 in
ASTM D-256
 10.7 J/cm
@Thickness 3.17 mm
20.0 ft-lb/in
@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 178 kJ/m²85.0 ft-lb/in²ASTM D-1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM D-648
 
Optical PropertiesMetricEnglishComments
Haze 6.0 %
@Thickness 3.17 mm
6.0 %
@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 76 %
@Thickness 3.17 mm
76 %
@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
 
Descriptive Properties
Bottle Means Failure Height, ft15+Vertical Free Fall; 30-g., 16-oz. cylinders
Equilibrium Torque, meter-grams1450Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Stability Time, minutes22

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Flexible P510 Natural Polyvinyl Chloride, Flexible
Teknor Apex APEX® 3202-90 Polyvinyl Chloride, Flexible
Colorite Polymers 9011G-015 (Extrustion), 9012G-015 (Molding) Radiation Sterilizable Vinyl Compound

PGGUL495 / 41771

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.