MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
ALIMEX ACP 6000 Aluminum Cast Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Aluminum cast plate ACP 6000 is a 7xxx series alloy surface-machined plate. This type of alloy ensures excellent machinability characteristics and adequate tensile strength. Thickness, flatness and surface finish offer very close tolerances.

Information provided by ALIMEX GmbH

Homogenized and stress relieved

Key Words: Al-Alloy type 7xxx
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.101 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 65
Tensile Strength, Ultimate 165 MPaRm
Tensile Strength, Yield 105 MPa
@Strain 0.2 %
Elongation at Break 3.0 %
Modulus of Elasticity 71.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000004778 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.5 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 984 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parkway Products Thixomolded® AM60A Magnesium
Magnesium AM60A-F, Die Cast
Alcoa MIC-6 Aluminum Mold Alloy
ALIMEX ACP 5080 Aluminum Cast Plate
Constellium Planoxal® 60 Aluminum plate

NALIMEX03 / 14758

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.