MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Label-Lyte™ 70LS447 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A two-side coated, shrink resistant, white, polypropylene film designed for use in hot melt cut-and stack labeling. It has an static resistant, matte finish, paper like print surface that is litho-printable, as well as compatible with water-based or solvent-based flexo and gravure inks and UV-cured inks. This film is deigned to be used as a monoweb and provides excellent converting performance, including printing, sheeting, guillotine cutting, and label transfer on magazine-fed labelers. The other side has a hot melt receptive coating.

Availability: Latin America, North America and South America

Key Features:

  • Excellent offset litho printing performance
  • Excellent static resistant properties for cut-and-stack labeling
  • Durable and moisture resistant
  • Excellent stiffness and burst performance
Features:
  • Static Resistant Coated
  • Static Resistant Matte Coated
Applications:
  • Beverage, Alcoholic
  • Beverage, Carbonated
  • Beverage, Mineral Waters
  • Dairy Products
  • Dry Foods and Beverage Powders
  • Household and Detergents
  • Industrial
Uses:
  • Cut & Stack (Hot Melt) Labels
Processing Method: Conventional Offset Lithography Printing, Digital Offset (HP Indigo) Printing, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, Thermal Transfer Printing, UV Flexographic Printing, UV Screen Printing and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3.00 milExxonMobil Method
Coating Weight 32.2 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 190 %20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 50 %20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, MD 13000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 24000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 5.5 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 5.5 %
@Temperature 135 °C
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Gloss 10 %45°, Print Surface; ExxonMobil Method
Transmission, Visible 15 %ExxonMobil Method
 
Descriptive Properties
Opacity90
Stiffness (Gurley)29 mgfMD
 50 mgfTD
Yield13400 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Label-Lyte® 187 LLG-102 Clear OPP Film
Borealis HC101BF Polypropylene Homopolymer
Borealis HB205TF Polypropylene
ExxonMobil Bicor™ 21MBT621 OPP Film
BP Amoco Amoco® 6361 Polypropylene Homopolymer

PEX99560 / 175796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.