Applications: Market: NOTE: Maximum process melt temperature is 265°F. PolyOne First Choice Disclaimer: Note: Pre-drying is recommended for 8-24 hours at 175°-185°F. NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation. |