MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aperam CuNi 44 Resistant Alloys Copper-Nickel Alloys
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: CuNi 44 presents the particularity to have a very low temperature coefficient, which makes it particularly interessant during its utilization in precision measurement testers. This is a very malleable, very ductile alloy, which presents a very good resistance to oxidation. CuNi 44 has also a very good solderability. Another field of application is manufacturing of thermocouples because it develops a high electromotive force (EMF) in association with others metals.

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 120
Tensile Strength 500 MPa
Tensile Strength, Yield 300 MPa
Elongation at Break >= 25 %on 100 mm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000049 ohm-cmTemperature coefficient = 0.000020/°C to 0.000060/°C from 20 - 100°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 21.1 W/m-K
@Temperature 120 °C
Melting Point 1210 °C
Maximum Service Temperature, Air 600 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 56 %
Nickel, Ni 44 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam CuNi 6 Resistant Alloys Copper-Nickel Alloys
Aperam CuNi 23 Resistant Alloys Copper-Nickel Alloys
Aperam CuNi 2 Resistant Alloys Copper-Nickel Alloys
Carlson 70 30 Cu Ni Copper-Nickel Alloy
Copper nickel 30%, UNS C71500

NPERA093 / 194882

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.