MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach Formadur® 2085 Plastic Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Description: FORMADUR 2085 is a free-machining corrosion-resistant mold frame steel

Characteristics: Lower mold production costs due to improved machinability; Improved corrosion resistance compared to Corroplast and Uniform hardness

Applications: Mold frames for processing corrosive plastics, Mold components and Plastic extrusion components

Heat Treatment: 1560°F- 1610°F; Cooling: Furnace 20°F/hour to 1200°F, Then air cools; Hardness: <230 HB

Information provided by Schmolz + Bickenbach

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 28
@Treatment Temp. 200 °C
 30
@Treatment Temp. 600.0 °C
 36
@Treatment Temp. 550.0 °C
 46
@Treatment Temp. 400 °C
 47
@Treatment Temp. 300 °C
 47
@Treatment Temp. 450 °C
 47
@Treatment Temp. 500 °C
 48
@Treatment Temp. 100 °C
Tensile Strength 160 ksi
@Temperature -5.56 °C
Hardened and tempered to 34 HRC
Tensile Strength, Yield 140 ksi
@Temperature 22.0 °C
Hardened and tempered to 34 HRC
Elongation at Yield 12 %
@Temperature 22.0 °C
Hardened and tempered to 34 HRC
Reduction of Area 45 %
@Temperature 22.0 °C
Hardened and tempered to 34 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.40 µin/in-°F
@Temperature 21.1 - 204 °C
Thermal Conductivity 163 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1830 - 1920 °FSoft; Hold at temperature for 30 min; Cooling: Oil; Quenched < 48 HRC
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.33 %
Chromium, Cr 16 %
Iron, Fe 83.12 %
Nickel, Ni 0.50 %
Sulfur, S 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel
Industeel Superplast® Stainless Mold Steel
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel
Industeel Superplast® 400 High Hardness Mold Steel
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel

NSCHMO007 / 125880

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.