Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a period of 20 minutes. Used as a protective sheath for wires and cables operating in interval of temperatures for -55°C to 70°C. Peculiarity of plastic is its good frost resistance. |