MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Borealis Borlink™ LE0550DC Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Borlink LE0550DC is a supersmooth crosslinkable black polyethylene compound, specially designed for semiconductive conductor screen and bonded insulation screen of power cables.

Applications: Borlink LE0550DC is intended for semiconductive screens of XLPE high voltage (HV) DC cables.

Specifications: Borlink LE0550DC is expected to meet the applicable requirements provided it is processed using sound material handling, extrusion and crosslinking practices as well as appropriate testing procedures.

Special Features: Borlink LE0550DC is a ready-to-use supersmooth semiconductive compound. The excellent distribution of carbon black additives in Borlink LE0550DC results in a superior smoothness of the semiconductive screen.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 15.0 MPa25 mm/min; ISO 527
Elongation at Break >= 200 %25 mm/min; ISO 527
 <= 10.0 %
@Pressure 0.200 MPa,
Temperature 200 °C
Permanent deformation; IEC 60811-507
 <= 100 %
@Pressure 0.200 MPa,
Temperature 200 °C
Elongation under load; IEC 60811-507
 >= 220 %
@Treatment Temp. 135 °C,
Time 605000 sec
IEC 60811-401
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 100 ohm-cm
@Temperature 23.0 °C
ISO 3915
 <= 1000 ohm-cm
@Temperature 90.0 °C
ISO 3915
 
Processing PropertiesOriginal ValueComments
Melt Temperature 120 - 130 °C
Shelf Life 18.0 Month
 
Descriptive Properties
Moisture Content100 pppmISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9648 / 323005

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.