MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Cast 3101 Encapsulating Adhesive System
Categories: Polymer; Thermoset; Epoxy

Material Notes: TRA-CAST 3101 is an easy-to-use, room temperature cure, rigid, low viscosity, 100% solids (no solvents) epoxy resin and hardener system with excellent mechanical and electrical properties. It is recommended for structural and electronic casting and encapsulating applications that require its excellent wetting and fluidity, good thermal expansion coefficients, and improved thermal shock resistance properties. TRA-CAST 3101 is readily mixed, handled and cured at room temperature, and it adheres to a wide range of materials including most metals, glass, ceramics and many plastics. Fully cured TRA-CAST 3101 is a strong, tough, durable electrical insulator which is also highly resistant to weather, water, gases and vapors, petroleum lubricants and fuels and many mild acids and alkalis.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccMixed
Viscosity 3000 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.40e+14 ohm-cm
 8.50e+10 ohm-cm
@Temperature 100 °C
Dielectric Constant 3.9
@Frequency 1e+6 Hz
 4.2
@Frequency 1000 Hz
Dielectric Strength 425 V/mil
Dissipation Factor 0.020
@Frequency 1000 Hz
 0.020
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -70.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 hour4 hrs @ 25°C + 2 hrs @ 65°C
 24.0 hour
@Temperature 25.0 °C
Pot Life 30 min
 
Descriptive Properties
Color Tan
Heat Distortion Temperature °C85
Mix Ratio, parts by weight100/125Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC100 / 71028

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.