MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kazanorgsintez Triethyleneglycol, Industrial
Categories: Fluid; Solvent

Material Notes: Production Method: Obtained by means of ethylene oxide irritation.

Application: Industrial triethylene glycol of A Grade is used as a feedstock for production of oligoetheracrylates, polyetheracrylates and plasticizers as well as other organic synthesis products

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  >= 1.121 g/cc
@Temperature 20.0 °C
>= 0.04050 lb/in³
@Temperature 68.0 °F
B Grade
 1.123 - 1.124 g/cc
@Temperature 20.0 °C
0.04057 - 0.04061 lb/in³
@Temperature 68.0 °F
A Grade
 
Component Elements PropertiesMetricEnglishComments
Free Water <= 0.10 %<= 0.10 %Grade A
 <= 0.30 %<= 0.30 %Grade B
 
Descriptive Properties
AppearanceClear liquid, free of mechanical impurities
Color180Hazen units, after boiling with hydrochloric acid, Grade A
 20Hazen units, Grade A
Mass Content (%)0.001Mass content of acids on conversion to acetic acid, Grade A
 0.005Mass content of peroxidates on conversion to iodine, Grade A
 0.01Mass content of aldehyde on conversion to acetaldehyde, Grade A
 0.1Mass content of monoethyleneglycol, Grade A
 0.8Mass content of monoethyleneglycol, Grade B
 10Mass content of sum of mono, di, and triethyleneglycol, Grade B
 2Mass content of sum of mono, di, and triethyleneglycol, Grade A
 90Mass content of triethylene glycol, Grade B
 98Mass content of triethylene glycol, Grade A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN142 / 127461

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.