MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pt-25% Ir Alloy, Annealed
Categories: Metal; Nonferrous Metal; Precious Metal; Platinum Alloy

Key Words: Platinum Iridium Alloy
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 21.66 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 240
Hardness, Knoop 282Estimated from Brinell
Hardness, Rockwell A 62Estimated from Brinell
Hardness, Rockwell B 100Estimated from Vickers
Hardness, Rockwell C 22Estimated from Brinell
Hardness, Vickers 247Estimated from Brinell
Tensile Strength, Ultimate 860 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000330 ohm-cmTemperature Coefficient = 0.00066/K (0-160°C)
 
Thermal PropertiesOriginal ValueComments
Melting Point 1845 °C
 
Component Elements PropertiesOriginal ValueComments
Iridium, Ir 25 %
Platinum, Pt 75 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pt-10% Ir Alloy, Annealed
Pt-3.5% Rh Alloy, Annealed
Pt-25% Ir Alloy, Hard
Pt-10% Ir Alloy, Hard
Pt-10% Rh Alloy, Annealed

MPPtI8 / 12573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.