MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MetalTek WASPALOY® Centri-Vac Nickel Cobalt Based Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Information provided by MetalTek

Key Words: Wrought UNS N07001; Wrought Grade WASPALOY®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.19 g/cc0.296 lb/in³Based on UNS number
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.2 - 1.5 %1.2 - 1.5 %
Carbon, C 0.030 - 0.10 %0.030 - 0.10 %
Chromium, Cr 18 - 21 %18 - 21 %
Cobalt, Co 12 - 15 %12 - 15 %
Molybdenum, Mo 3.5 - 4.0 %3.5 - 4.0 %
Nickel, Ni 55.15 - 62.52 %55.15 - 62.52 %
Titanium, Ti 2.75 - 3.25 %2.75 - 3.25 %
 
Descriptive Properties
Heat TreatmentSol. Anneal & Age

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Waspaloy A Nickel Superalloy (UNS N07001)
Waspaloy B Nickel Superalloy
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Special Metals NIMONIC® Alloy 80A
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age

NMETEK157 / 18407

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.