MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Purell HP671T Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Purell HP671T is a nucleated polypropylene homopolymer with a gamma – ray stabilizing additive for usage in injection molding applications. Purell HP671T exhibits very high stiffness combined with an excellent transparency. Purell HP671T is typically used in rigid, high transparency pharmaceutical and diagnostic applications. Applications: Diagnostic Applications, Healthcare Applications, Lab ware, Medical Devices, Syringes.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 55 g/10 min
@Load 2.16 kg,
Temperature 230 °C
55 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 72.0 MPa10400 psiISO 2039-1
Tensile Strength, Yield 39.0 MPa5660 psiISO 527-1,-2
Elongation at Break >= 16 %>= 16 %ISO 527-1,-2
Elongation at Yield 7.5 %7.5 %ISO 527-1,-2
Tensile Modulus 1.90 GPa276 ksiISO 527-1,-2
Charpy Impact, Notched 0.260 J/cm²
@Temperature 23.0 °C
1.24 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 155 °C311 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 18 %18 %
Gloss 125 %125 %@ 45°; ASTM D2457
 
Descriptive Properties
Ball Indentation Hardness (MPa)H358/30
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
Avient Nanoblend™ LST 5501 Polypropylene
Avient Maxxam™ DP 4980-1-1000 Polypropylene Homopolymer (PP Homopolymer)
Avient Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer)
A. Schulman Diamond NPP30-2000HC Homopolymer Polypropylene

PEQT8630 / 220264

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.