MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat PLUS® 301 A FR Polycarbonate (PC), ESD Protection - Permanently Static Dissipative - Glass Fiber - Flame Retardant - Preliminary Datasheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D 792
Additive Loading 10 %10 %Primary Additive
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 2.0 - 5.0 %2.0 - 5.0 %ASTM D 638
Tensile Modulus 3.45 GPa500 ksiASTM D 638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 - 9.90e+8 ohm-cm1.00e+7 - 9.90e+8 ohm-cmASTM D 257
Surface Resistivity per Square 1.00e+8 - 9.90e+9 ohm1.00e+8 - 9.90e+9 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 - 243 °C430 - 470 °F
Mold Temperature 65.6 - 121 °C150 - 250 °F
Drying Temperature 121 °C
@Time 14400 sec
250 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 41.4 - 68.9 MPa6000 - 10000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TW441 Nylon 46 (European and Asian Grade) (Cond)
Envalior Stanyl® TW341 PA46, Dry, Heat Stabilized
BASF Ultramid® A3W Q601 PA66 (Dry)
BASF Ultramid® A3K PA66 (Dry)
BASF Elastollan® C-90A Polyester Type Polyurethane Elastomer

PQZQA40510 / 239945

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.