MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled; Nylon 6, Heat Stabilized; Nylon 6, Impact Grade

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Moisture Absorption 2.30 %
@Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cmEurotec
Linear Mold Shrinkage, Transverse 0.014 cm/cmEurotec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPaISO 527
Elongation at Break 4.0 %ISO 527
Tensile Modulus 5500 MPaISO 527
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 65.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1U
 75.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Comparative Tracking Index 500 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 223 °C[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 200 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 185 °CISO 75
Flammability, UL94 HB
@Thickness 0.750 mm
 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 270 °C
Feed Temperature 60.0 - 80.0 °CThroat
Mold Temperature 60.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.20 %ISO 960
Hold Pressure 50.0 - 100 MPa
 
Descriptive Properties
Back PressureLow
Injection SpeedFast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Envalior Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced
E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM

PEUROS057 / 147047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.