MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon R38041X012 0.012" (0.305 mm) Uncured Fluorosilicone with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Interleave 1: Polyethylene
Side 1: Uncured Silicone Rubber
Substrate: Style 2116 Fiberglass
Side 2: Uncured Silicone Rubber
Interleave 2: Polyethylene

Appearance: Gray silicone gum and on fiberglass cloth

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.81 g/ccFluorosilicone Property; Arlon SQA-TMS-024
Thickness 2.50 milInterleave 1
 2.50 milInterleave 2
 4.00 milSide 1; Arlon SQA-TMS-003
 4.00 milSide 2; Arlon SQA-TMS-003
 4.00 milSubstrate; Arlon SQA-TMS-003
 12.0 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65Fluorosilicone Property; ASTM D2240
Tensile Strength 558 psiFluorosilicone Property; ASTM D412
Elongation at Break 82 %Fluorosilicone Property; ASTM D412
Tear Strength 28.0 pliDie B, Silicone Property; ASTM D624
Peel Strength 1.10 pliBond Strength; Arlon SQA-TMS-011
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 204 °C
Recommended Postcure Cycle
 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 21.1 °C
From date of manufacture
 
Descriptive Properties
ColorDark Gray
 WhiteSubstrate
Fuel Resistance11.9Fuel CM85 Resistance, ASTM D471
 18.7Fuel C Resistance, ASTM D471
 6Fuel A Resistance, ASTM D471
Total Product Weight (oz/yd2)13.4Arlon SQA-TMS-025, Product Property
 81.4Arlon SQA-TMS-025, Fluorosilicone Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier
Precision Polymer Engineering F80X Fluorosilicone Rubber
Precision Polymer Engineering F50A Fluorosilicone Rubber
P & P Technology EC-Q(F) Fluorosilicone Elastomer
NuSil CF2-3521-2 Fluorosilicone

PARL671 / 125857

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.