MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 5010H High Density Polyethylene, High Molecular Weight
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: This resin is a high molecular weight, high density copolymer polyethylene resin. This resin exhibits superior impact strength and ESCR and contains a process stabilizer. This product meets US FDA 21 CFR 177.1520.

Applications: Blow Molding Applications; Drums; Fuel Tanks; Jerricans

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: High ESCR (Stress Crack Resist.); High Impact Resistance; High Molecular Weight
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccASTM D-792
ESCR 100% Igepal® 600 hourASTM D-1693
Melt Flow 10 g/10 minASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.4 MPaASTM D-638
Flexural Modulus 1.241 GPaASTM D-790
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processBlow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BL2631 High Density Polyethylene
Amco PRIMATOP HDPE 002955 Phillips Process Hexene Copolymer
Bamberger Polymers Bapolene® 3042U Polyethylene, Rotational Molding Grade
Borealis BL0521 High Density Polyethylene
Borealis BL1481 High Density Polyethylene

PBP1109 / 81001

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.