MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CEN® Electronic Material HT Polyimide Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: CEN® HT is a one side or both sides electrically conductive polyimide film for heating applications. With precisely controlled surface resistivity, the film resistive property is retained throughout the film, so it cannot be cracked, rubbed off or easily damaged, as is often the case with surface coatings or metallizations.

Applications: heaters, heating facilities for automotive, health care, agriculture, aerospace, and consumer electronics.

All information provided by CEN Electronic Material Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/cc
Thickness 46.0 - 54.0 micronsASTM D374
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 110 MPaASTM D882
Film Tensile Strength at Yield, TD 100 MPaASTM D882
Elongation at Yield >= 10 %ASTM D882
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 10000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 1.25 Month
 
Descriptive Properties
Folding Endurance>500,000 times
Power Density (W/cm²)6
Rate of Electricity to Thermal (%)>99
Tolerance of Resistance (%)<3
Working Voltage (V)3-850

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CEN® Electronic Material CF 120CF616 Polyimide Film
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness
Overview of materials for Polyimide, Thermoset Film
CEN® Electronic Material BX Polyimide Film
CEN® Electronic Material CN Polyimide Film, 5 Mil Thickness

PCENE002 / 93464

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.