MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M76/M55J Curing Epoxy Matrix with Fibers
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 36.0 MPa5220 psi90°
 2157 MPa312800 psi
Tensile Modulus 6.50 GPa943 ksi90°
 338 GPa49000 ksi
Flexural Strength 1186 MPa172000 psi
 951 MPa
@Temperature 121 °C
138000 psi
@Temperature 250 °F
0°, Wet
Flexural Modulus 296 GPa42900 ksi
 286 GPa
@Temperature 121 °C
41500 ksi
@Temperature 250 °F
0°, Wet
Compressive Strength 1048 MPa152000 psi
Compressive Modulus 0.298 GPa43.2 ksi
Shear Strength 81.0 MPa11700 psiInterlaminar, 0°
 60.0 MPa
@Temperature 121 °C
8700 psi
@Temperature 250 °F
Interlaminar, 0°, Wet
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9149 / 322305

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.