MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® PFA P62X Orange Pigmentation
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: (Perfluoroalkoxy) for pigmentation. The color concentrates are based on Fluon® PFA P-62X and are supplied in cylindrical pellet form. These pellets are approximately 0.125” long by 0.080” diameter.

End Uses: Colored injection molded parts, film, tubing, colored wire or jacket insulation where a pigmented appearance is required.

Information provided by AGC Chemicals Americas Inc.

Key Words: 442-015-665
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.20 g/cc0.0434 lb/in³
Melt Flow 27 g/10 min27 g/10 min
ASTM Color 4040a, CIELAB, 10° obs., D65
 50.350.3b, CIELAB, 10° obs., D65
 56.956.9L, CIELAB, 10° obs., D65
 
Descriptive Properties
Dispersion Quality0.0015 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® FC168-63 PTFE, 63% Bronze and Graphite Filled
Afton Plastics 450HP PFA Welding Rod
AGC Fluon® FP-EF-101 PTFE, 5% Glass Filled
AGC Fluon® FC100-25 1000 PTFE, 25% Glass Fiber Filled
AGC Fluon® FC 15 MIN PTFE, 15% Wollastonite Filled

PAGCX234 / 191343

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.