MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Meilian Chemical W9350 WHITE MASTERBATCH  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: W9350 is a LDPE based masterbatch designed for use in film products for general purpose.

Method of Usage: W9350 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, free from pollution problem caused by pigment.

Range of Application: W9350 is designed for applications of injection molding, blow film and legging in LDPE, HDPE, LLDPE, and PP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.98 g/cc
Melt Index of Compound 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
 
Descriptive Properties
CarrierLDPE
CompatibilityLDPE, HDPE, PP and Ethylene copolymer
Pigment Content: TiO2 (%)47

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOMER® FR 100 Additive
Lubrizol Advanced Materials Pearlthane® MB-9010 Thermoplastic Polyurethane Elastomer
Meilian Chemical PE12077 WHITE MASTERBATCH
Meilian Chemical PE105B WHITE MASTERBATCH
ExxonMobil Univis HVI 13

PMEILI04 / 52749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.