MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Parker Chomerics CHO-FORM 5526 EMI Shielding Material
Categories: Polymer; Adhesive

Material Notes: Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material cost versus performance and can provide low cost alternatives for less demanding applications. Chomerics corrosion resistant materials inherently provide protection against galvanic activity. They may eliminate the need for nickel or tin plating and or secondary environmental gaskets. Chomerics general purpose materials exhibit excellent electrical and mechanical properties on metallic and shield plastic housing. Chomerics silver filled materials provide high shielding and conductivity critical for inter-compartmental shields. CHOFORM delivers a greater deflection range, lower deflection forces & improved reliability.

Features: Lower deflection forces and a broad deflection range, Corrosion resistant materials can eliminate plating or secondary environmental gasket, Good adhesion to many substrates, Supply chain management providing ongoing logistics, Low cost and rapid prototyping and High conductivity, Excellent Grounding and Shielding.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.60 g/cc3.60 g/ccASTM D792
Deformation 30 %30 %26.3 N/cm; ASTM D575 Modified
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838ASTM D2240
Tensile Strength at Break 0.552 MPa80.0 psiASTM D412
Elongation at Break 75 %75 %ASTM D412
Compression Set 45 %
@Temperature 70.0 °C,
Time 79200 sec
45 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0030 ohm-cm0.0030 ohm-cmChomerics MAT-1002
Shielding Effectiveness >= 100 dB
@Frequency 2.00e+8 - 1.20e+10 Hz
>= 100 dB
@Frequency 2.00e+8 - 1.20e+10 Hz
Modified IEEE-299
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 85.0 °C185 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  18.0 min
@Temperature 22.0 °C
0.300 hour
@Temperature 71.6 °F
50% RH; Handling Time
 1440 min
@Temperature 22.0 °C
24.0 hour
@Temperature 71.6 °F
50% RH; Full Cure
Tack-Free Time 240 min
@Temperature 22.0 °C
4.00 hour
@Temperature 71.6 °F
50% RH
Shelf Life 6.00 Month
@Temperature 17.0 - 27.0 °C
6.00 Month
@Temperature 62.6 - 80.6 °F
Chomerics
 
Descriptive Properties
Adhesion9 N/cmTrivalent Chromate Coating on Al, Chomerics WI 1038
Cure MechanismMoisture
FillerAg
Number of Components1
Resin SystemSilicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-FORM 5532 EMI Shielding Material
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
NuSil EPM-2463 Silicone, Thermal Interface Material (TIM): Electrically Conductive
NuSil R-2634 Silicone, Electrically Conductive
P & P Technology EC-S Pure Silver Loaded Silicone

PCHOME084 / 28306

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.