MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 3150 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 3100 series are engineered materials designed primarily general purpose, automotive and industrial applications requiring a good balance of thermal, mechanical, and physical properties. Sarlink 3150, available in NAT and BLK, is a medium hardness, low density, multi-purpose thermoplastic vulcanizate that can be processed by injection molding, blow molding or extrusion for applications such as grips, seals, gaskets, profiles, hose & tubes, bellows, and other articles.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Flexibility; Good Moldability; Good Processability; Good Surface Finish; High Elasticity; Medium Heat Resistance; Low Density; Medium Hardness; Low Specific Gravity; Resilient; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Automotive Under the Hood; Diaphragms; Gaskets; General Purpose; Industrial Applications; O-rings; Profiles; Rubber Replacement; Seals; Weatherstripping

RoHS Compliance: RoHS Compliant

Automotive Specifications: CHRYSLER MS-AR-80 Type A Color: Black; CHRYSLER MS-AR-80 Type A Color: Natural; GM QK 003533 Color: Black; GM QK 003533 Color: Natural; PSA Peugeot-Citroen SPA Color: Black; RENAULT F.R.M. 6A 05 A08 Color: Black; VAG VW501 23 Color: Black; VAG VW501 79 Color: Black; VOLKSWAGEN VW 50180 Color: Black

Agency Ratings: UL 94

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Viscosity 270 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 54
@Time 5.00 sec
Extruded; ISO 868
 56
@Time 5.00 sec
Injection Molded; ISO 868
Tensile Strength at Break 470 psiAcross Flow; ISO 37
 595 psiFlow; ISO 37
 442 psi
@Treatment Temp. 135 °C,
Time 360000 sec
Across Flow, Change in Air; ISO 188
 503 psi
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain 276 psi
@Strain 100 %
Across Flow; ISO 37
 435 psi
@Strain 100 %
Flow; ISO 37
 290 psi
@Strain 100 %,
Treatment Temp. 150 °C
Across Flow, Change in Air, 168 hr; ISO 188
 295 psi
@Strain 100 %,
Treatment Temp. 135 °C
Across Flow, Change in Air, 1000 hr; ISO 188
Elongation at Break 240 %Flow; ISO 37
 600 %Across Flow; ISO 37
 558 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
Across Flow, Change in Air; ISO 188
 648 %
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
Tear Strength 140 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set 20 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 32 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 52 %
@Temperature 90.0 °C,
Time 252000 sec
ISO 815
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 122 °FUL 746
UL RTI, Mechanical with Impact 122 °FUL 746
UL RTI, Mechanical without Impact 122 °FUL 746
Flammability, UL94 HB
@Thickness 1.52 mm
All Colors
 
Processing PropertiesOriginal ValueComments
Processing Temperature 365 - 428 °FInjection, Melt
Rear Barrel Temperature 356 - 419 °FInjection
Middle Barrel Temperature 356 - 419 °FInjection
Front Barrel Temperature 356 - 419 °FInjection
Nozzle Temperature 369 - 428 °FInjection
Zone 1 356 - 392 °FExtrusion
Zone 2 356 - 401 °FExtrusion
Zone 3 369 - 410 °FExtrusion
Zone 4 369 - 410 °FExtrusion
Die Temperature 383 - 419 °FExtrusion
Melt Temperature 383 - 419 °FExtrusion
Mold Temperature 50.0 - 131 °FInjection
Drying Temperature 180 °F
Dry Time 3.00 hour
Back Pressure 14.5 - 145 psiInjection
Screw Speed 100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1141 / 237632

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.