MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound GF004 Polysulfone (PSU) (Americas)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: LNP THERMOCOMP GF004 compound is based on Polysulfone (PSU) resin containing 20% glass fiber.

Features: High Stiffness,Structural

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
 1.41 g/ccASTM D792
Moisture Absorption 0.0500 %Injection Molding
 0.100 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm24hrs; ASTM D955
 0.0064 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0085 cm/cm24hrs; ISO 294
 0.0090 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 91.0 MPaASTM D638
Tensile Strength, Yield 91.0 MPaASTM D638
Elongation at Break 2.3 %ASTM D638
Elongation at Yield 2.3 %ASTM D638
Tensile Modulus 6200 MPa50 mm/min; ASTM D638
Flexural Strength 137 MPaASTM D790
 145 MPaISO 178
Flexural Modulus 6000 MPaISO 178
 6200 MPaASTM D790
Izod Impact Notched 53.0 JASTM D256
Izod Impact, Unnotched 427 J/mASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 Jpeak; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 25.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 52.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 52.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 180 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 178 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 174 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 173 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 340 - 350 °C
Zone 3 350 - 360 °C
Melt Temperature 360 - 370 °CInjection Molding
Mold Temperature 150 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81603 / 289550

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.