MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mo-Sci Corporation GL 1742 Glass-ceramic
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: Applications : To seal ceramics and metals . Sealing glasses function as high-temperature sealant materials for solid oxide fuel cells (SOFCs) and other applications such as sodium-ion batteries.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.80 g/cc
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.50 µm/m-°C
@Temperature 50.0 - 500 °C
Transformation Temperature, Tg 660 °C+/- 10°C
Softening Point 693 °CDilatometric +/- 10°C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 760 °C
@Time 7200 sec
Firing Temp. Step 1. Heating/cooling rate: 3 to 10°C/min
 830 °C
@Time 7200 sec
Firing Temp. Step 2
 
Component Elements PropertiesOriginal ValueComments
Al2O3 1.61 - 3.61 %
B2O3 2.56 - 4.56 %
SiO2 29.29 - 35.29 %
 
Descriptive Properties
Tc830°C+/- 10°C
ZnO (%)25.07 to 29.07

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Advanced Ceramics ACL 2088 Zinc Alumino-Silicate
Accuratus MACOR Machinable Glass Ceramic
Corning Pyroceram® Code 9606 Glass Ceramic
Mateck Zero Expansion Glass - ZERODUR
712-3 Nextrema® Tinted Glass Ceramic/SCHOTT

CMOSCI9006 / 200221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.