MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Röchling Glastherm® HT 500 Heat Insulation component
Categories: Polymer; Thermoset

Material Notes: Glastherm® HT 500 has an extremely high level of heat resistance, making it suitable for processes with a continuous working temperature of up to 500°C (932°F). The material also has an excellent load capacity in high temperature and a very good level of resistance to thermal shock. Glastherm® HT 500 is incombustible, free of asbestos and can be easily cut and adapted with standard metal tools.
  • Maximum continuous operation temperature: 500°C (932°F)
  • High compressive strength: 300 MPa (at 200°C)
  • Good thermal insulation

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.15 g/cc0.0777 lb/in³ISO 1183
Water Absorption <= 0.50 %<= 0.50 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 230 MPa33400 psiISO 178
Compressive Strength  300 MPa
@Temperature 200 °C
43500 psi
@Temperature 392 °F
20x20x20 mm; ISO 604
 400 MPa
@Temperature 23.0 °C
58000 psi
@Temperature 73.4 °F
Perpendicular, 20x20x20 mm; ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C5.56 µin/in-°FParallel
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FPerpendicular
Maximum Service Temperature, Air 500 °C932 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9125 / 232828

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.