MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated additive package consists of a high level antiblocking agent and a medium level slip agent to guarantee a low coefficient of friction (COF), which is fundamental for improved machinability in overwrap applications. This product is identified as PE 123 according to ASTM D-4976-04a standard specification. Its applications include: films for automatic overwrap packaging of hygiene markets [toilet tissue, kitchen paper, and napkin (paper products) overwrap], laminated films for food packaging with PP or BOPP (coffee, crackers, and powder milk), and films which require good optical proprieties aligned with high stiffness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.931 g/ccASTM-D792
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 400 %ASTM-D882
Film Elongation at Break, TD 670 %ASTM-D882
Secant Modulus, MD 0.190 GPa2% Secant Modulus; ASTM-D882
Secant Modulus, TD 0.170 GPa2% Secant Modulus; ASTM-D882
Elmendorf Tear Strength MD 280 gASTM-D1922
Elmendorf Tear Strength TD 380 gASTM-D1922
Elmendorf Tear Strength, MD 5.60 g/micronASTM-D1922
Elmendorf Tear Strength, TD 7.60 g/micronASTM-D1922
Dart Drop 2.40 g/micronASTM-D1709
Dart Drop Test 120 gASTM-D1709
Film Tensile Strength at Break, MD 20.0 MPaASTM-D882
Film Tensile Strength at Break, TD 18.0 MPaASTM-D882
 
Optical PropertiesOriginal ValueComments
Haze 10 %ASTM-D1003
Gloss 60 %Angle 45°; ASTM-D2457
 98 %Angle 60°; ASTM-D2457
 
Processing PropertiesOriginal ValueComments
Die Opening 0.100 cmBlow Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.0Blow Film Extrusion
 
Descriptive Properties
Mass Temperature (°C)170-180Blow Film Extrusion
Temperature Profile (°C)150-180Blow Film Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer
A. Schulman Diamond NPP10-0218 Low Density Polyethylene
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin
Celanese 520 Film LDPE polymer for flexible packaging

PBRAS835 / 106681

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.