MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Idemitsu Kosan TARFLON™ AC1070C Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: High flow.

Polycarbonate is known for its high impact resistance, good transparency and heat resistance, and superb precision and electrical properties. TARFLON is used in a wide range of applications such as house wares, office equipment , mobile devices, communications equipment, display devices such as LCD backlight parts, automotive, lighting and many fields.

Information provided by Idemitsu Losan Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183(JIS K7112)
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 2.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.0787 in
Idemitsu Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 2.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.0787 in
Idemitsu Method
Melt Flow 25.62 g/10 min
@Load 2.16 kg,
Temperature 280 °C
25.62 g/10 min
@Load 4.76 lb,
Temperature 536 °F
ISO 1133 (JIS K7210)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiISO 527-1,2 (JIS K7161, 7162)
Elongation at Break 80 %80 %Nominal; ISO 527-1,2 (JIS K7161, 7162)
Flexural Strength 93.0 MPa13500 psiISO 178 (JIS K7171)
Flexural Modulus 2.90 GPa421 ksiISO 178 (JIS K7171)
Charpy Impact, Notched 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1(JIS K7111)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FISO 75-1,2 (JIS K7191-1,2)
Deflection Temperature at 1.8 MPa (264 psi) 116 °C241 °FISO 75-1,2 (JIS K7191-1,2)
UL RTI, Electrical 80.0 °C176 °FUL746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL746B
Flammability, UL94  V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °FCylinder Temperature
 <= 290 °C<= 554 °FMax Cylinder Temperature
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 120 °C
@Time 18000 - 28800 sec
248 °F
@Time 5.00 - 8.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIDEM218 / 249582

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.