Product Description: EA55-003 is an unstabilized blow molding grade high density polyethylene copolymer. The base resin can be compounded to incorporate such things as stabilizers, fillers, and colorants before processing in order to meet the needs of the specific molding application. Availability: Latin America, North America and South America Additive: - Thermal Stabilizer: Yes
- Antistatic: No
Applications: Information provided by ExxonMobil Chemical |