REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punches, die inserts, and cutting applications involving high speeds and light cuts. It is designed to give maximum performance working with abrasive materials, exhibiting better wear resistance than M2 or M3.Information provided by Crucible Industries |