MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® KT-820 SL45 PEEK, Very good wear resistance
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Very good wear resistance, lubricated, injection molding

KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.

Markets/Uses: Automotive / Air Induction / Air Pump Impeller; Automotive / Drivetrain / Lubricated; Automotive / Drivetrain / Seal Rings; Automotive / Drivetrain / Thrust Washers; Automotive / Mechanical & Structural Parts / Gears; Oil & Gas / Down Hole / Bushings and Bearings; Wear-Resistant Plastics / High Temperature Friction & Wear / Bearings; Wear-Resistant Plastics / High Temperature Friction & Wear / Gears; Wear-Resistant Plastics / High Temperature Friction & Wear / Lubricated

Applications: Automotive Applications; Bushings; Gears; Oil/Gas Applications; Thrust Washer

Features: Chemical Resistant; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; Wear Resistant

Injection notes: Back Pressure: minimum

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccASTM D792
Water Absorption 0.030 %
@Time 86400 sec
ASTM D570
Viscosity 380 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow <= 0.0020 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.013 - 0.015 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ASTM D785
Tensile Strength 161 MPaASTM D638
Tensile Strength, Yield 197 MPaType 1A, 5 mm/min; ISO 527-2
Elongation at Break 1.5 %5.0 mm/min; ASTM D638
 1.5 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 18300 MPaASTM D638
 25300 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 265 MPaASTM D790
 273 MPaISO 178
Flexural Modulus 16600 MPaASTM D790
 24100 MPaISO 178
Compressive Strength 127 MPaASTM D695
Shear Strength 84.1 MPaASTM D732
Izod Impact, Notched 69.0 J/mASTM D256
Izod Impact, Unnotched 530 J/mASTM D256
Izod Impact, Notched (ISO) 8.50 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 43.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Specific Heat Capacity 1.25 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.67 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.360 W/m-KASTM C177
Melting Point 342 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 299 °CAnnealed; ASTM D648
Glass Transition Temp, Tg 152 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 366 °C
Middle Barrel Temperature 371 °C
Front Barrel Temperature 377 °C
Nozzle Temperature 382 °C
Mold Temperature 177 - 204 °C
Drying Temperature 149 °C
@Time 14400 sec
 
Descriptive Properties
AdditiveCarbon Fiber + PTFE Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4323 / 280123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.