MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Tribocomp® PA66 GF40 TS5 Glass / Aramid fibers reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Glass / Aramid fibers reinforced, high flow PA

Tribocomp® PA66 GF40 TS5 is high-flow PA compound reinforced with a specific package of glass and aramid fibers, which results in unique properties. The grade can easily be processed on most injection molding machines.

Applications: Automotive Applications; Consumer Applications; Industrial Applications

Features: High Flow; High Stiffness; High Strength

The value listed as Molding Shrinkage ISO 294-4, was tested in accordance with S.O.P. methods.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
Moisture Absorption 1.20 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPa
@Temperature 120 °C
ISO 527-2
 185 MPa
@Temperature 23.0 °C
ISO 527-2
Elongation at Break 2.4 %ISO 527-2
Tensile Modulus 12500 MPaISO 527-2
Flexural Strength 255 MPaISO 178
Flexural Modulus 11500 MPaISO 178
Charpy Impact Unnotched 48.0 kJ/m²ISO 179
Charpy Impact, Notched 12.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+12 ohmASTM D257
Dielectric Strength 37.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 27.0 µm/m-°CISO 11359-2
Thermal Conductivity 0.310 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 252 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 270 - 300 °C
Middle Barrel Temperature 275 - 295 °C
Front Barrel Temperature 280 - 295 °C
Nozzle Temperature 290 - 310 °C
Melt Temperature <= 300 °CInjection
Mold Temperature 80.0 - 130 °C
Drying Temperature 80.0 °C
@Time 14400 sec
Moisture Content <= 0.10 %Injection
 
Descriptive Properties
AvailabilityEurope
ColorNatural Color
FormsPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4560 / 280360

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.