MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Total Xsene® XS10 B HDPE, pipe, injection molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: FINATHENE® XS10 B is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™.

FINATHENE® XS10 B is a high performance black compound specially developed for potable water and gas distribution applications.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³ASTM D 792
Viscosity  270000 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
270000 cP
@Shear Rate 1000 1/s,
Temperature 374 °F
ATOFINA research test
 2.10e+6 cP
@Shear Rate 100 1/s,
Temperature 190 °C
2.10e+6 cP
@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Oxidative Induction Time (OIT) >= 20 min>= 20 min200°C; EN 728
 >= 20 min>= 20 min210°C; EN 728
Carbon Black Loading 2.0 - 2.5 %2.0 - 2.5 %ISO 6964
Melt Flow 0.30 g/10 min
@Load 5.00 kg
0.30 g/10 min
@Load 11.0 lb
ISO 1133
High Load Melt Index 8.0 g/10 min
@Load 21.6 kg
8.0 g/10 min
@Load 47.6 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psiISO 527
Tensile Strength, Yield 26.0 MPa3770 psi
Elongation at Break >= 700 %>= 700 %ISO 527
Elongation at Yield 9.0 %9.0 %ISO 527
Flexural Modulus 1.10 GPa160 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 2.00 J/g-°C0.478 BTU/lb-°FDSC
 2.60 J/g-°C
@Temperature 150 °C
0.621 BTU/lb-°F
@Temperature 302 °F
DSC
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FDIN 52612
 0.200 W/m-K
@Temperature 150 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 302 °F
DIN 52612
Melting Point 130 - 132 °C266 - 270 °Fcrystalline; DSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostalen CRP 100 BLACK (XL) High Density Polyethylene (HDPE), Pipe Grade
Ethydco Advancene™ bEE-4906-AAH HDPE Pipe Extrusion
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Total Xsene® XS10 H HDPE, pipe, injection molding
Borealis BL0521 High Density Polyethylene

PFINAP122 / 38705

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.