MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRILOY™ Compound D20001 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRILOY D20001 compound is based on Polycarbonate (PC) resin containing proprietary lubricant. Added features of this grade include: Non-Brominated, Non-Chlorinated Flame Retardant, Wear Resistant.

Features: Flame Retardant,Wear resistant,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
 1.20 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.120 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm24hrs; ASTM D955
 0.0053 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0057 cm/cm24hrs; ISO 294
 0.0060 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPaISO 527
 60.0 MPaASTM D638
Tensile Strength, Yield 62.0 MPaISO 527
 67.0 MPaASTM D638
Elongation at Break 6.5 %ASTM D638
 6.7 %ISO 527
Elongation at Yield 4.3 %ISO 527
 4.5 %ASTM D638
Tensile Modulus 2550 MPa50 mm/min; ASTM D638
 2600 MPa1 mm/min; ISO 527
Flexural Strength 102 MPaISO 178
 103 MPaASTM D790
Flexural Modulus 2800 MPaISO 178
 2820 MPaASTM D790
Izod Impact Notched 64.0 JASTM D256
Izod Impact, Unnotched 1612 J/mASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 104 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 51.0 Jpeak; ASTM D3763
Coefficient of Friction, Dynamic 0.29ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.16ASTM D3702 Modified: Manual
K (wear) Factor 10.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index >= 600 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 65.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 66.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 89.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness 0.500 mm
UL 94
 V-2
@Thickness 0.800 mm
UL 94
 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 255 - 265 °C
Zone 3 260 - 270 °C
Melt Temperature 255 - 290 °CInjection Molding
Mold Temperature 40.0 - 65.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81127 / 289074

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.