MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik Polymer OH 0.08
Categories: Polymer

Material Notes: Polymer OH are polydimethyl siloxanes with terminal silanol groups used as base polymers in condensation-curing silicone elastomers. Polymer OH is available in different viscosity levels between 80 and 400 000 mPas. Other viscosities are possible upon request. Please note that Polymer OH 0,08 acts as an inhibitor and can therefore be used for delaying the curing process.

Application: Polymer OH can be cured with usual condensation crosslinkers such as alkoxy silanes, acetoxy silanes (Crosslinker AC), oxime silanes (Crosslinker Ox and Crosslinker OX MOD) and enoxy silanes (Crosslinker K) in connection with catalysts (e. g. tin catalysts, Catalyst TD 18). Especially the low-viscosity types can be used as reactive diluents for the viscosity adjustment in a mixture with higher viscosity polymers. The crosslinking reaction occurs in connection with water. In conventional single-component formulations, this water can be introduced through humidity. However, Polymer OH can also be formulated as two component systems. In that case, the required water is added through the second component. Substantially higher curing rates and depths are achieved in this way.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/inĀ³
Viscosity 80 cP80 cP
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.40581.4058
 
Descriptive Properties
Appearanceclear, colorless liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIM076 / 197280

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.