MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Colour Image Plastic Compound Mineralblend® PP-2800 PP, 40% Mica Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Mica Filler

Material Notes: Product Description: Mineralblend® PP-2800 is a medium flow mica filled homopolymer polypropylene compounds characterized by high stiffness and dimensional stability with additional low shrinkage properties.

Features:

  • Mica filled, 40%
  • Low shrinkage
  • High stiffness
  • High dimensional stability
Uses:
  • Appliances Applications
  • Electrical/Electronic Parts
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 30.0 MPaASTM D638
Elongation at Break 10 %ASTM D638
Flexural Strength 52.0 MPaASTM D790
Flexural Modulus 5400 MPaASTM D790
Izod Impact, Notched 40.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
@Thickness 4.00 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
@Thickness 4.00 mm
Unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 180 - 190 °C
Middle Barrel Temperature 190 - 200 °C
Front Barrel Temperature 200 - 210 °C
Nozzle Temperature 210 - 220 °C
Melt Temperature 190 - 220 °C
Mold Temperature 60.0 - 70.0 °C
Drying Temperature 100 °C
Dry Time 2.00 hour
 <= 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOLO044 / 265936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.