MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel; Mold Steel

Material Notes: Description: DH2F is one of the best machining pre-hardened H13-type steels available.

Unique Characteristics:

  • 38-42 HRc hardness.
  • Through hardened for exceptional dimensional stability.
  • Cuts mold making costs by reducing man hours required for machining. Classified as a “free-machining” steel.
  • Ideal for complex, precision molds and parts susceptible to distortion and/or deformation without needing additional heat-treating.
  • Ideal for Ion-nitriding.

Applications:

  • Molds for plastics
  • Diecast die components
  • Plunger tips, sprue bushings
  • Diecasting dies for aluminum and zinc
  • Dies for aluminum extrusions
  • Press dies
  • Dieplate strippers
  • Machine parts

Information provided by International Mold Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 38 - 42
Hardness, Vickers 130
@Temperature 700.0 °C
 220
@Temperature 600.0 °C
 320
@Temperature 300 °C
 320
@Temperature 400 °C
 320
@Temperature 500 °C
 330
@Temperature 200 °C
 380
@Temperature 100 °C
 400
@Temperature 23.0 °C
Tensile Strength, Ultimate 400 MPa
@Temperature 700.0 °C
 785 MPa
@Temperature 600.0 °C
 1080 MPa
@Temperature 500 °C
 1100 MPa
@Temperature 400 °C
 1170 MPa
@Temperature 300 °C
 1300 MPa
@Temperature 200 °C
 1300 MPa
@Temperature 23.0 °C
Tensile Strength, Yield 300 MPa
@Temperature 700.0 °C
 730 MPa
@Temperature 600.0 °C
 850 MPa
@Temperature 400 °C
 880 MPa
@Temperature 500 °C
 1050 MPa
@Temperature 300 °C
 1100 MPa
@Temperature 200 °C
 1100 MPa
@Temperature 23.0 °C
Elongation at Break 10 %
@Temperature 23.0 °C
 10 %
@Temperature 392 °C
 10 %
@Temperature 752 °C
 12 %
@Temperature 572 °C
 13 %
@Temperature 932 °C
 20 %
@Temperature 1112 °C
 37 %
@Temperature 1292 °C
Reduction of Area 15 %
@Temperature 23.0 °C
 22 %
@Temperature 400 °C
 25 %
@Temperature 200 °C
 26 %
@Temperature 300 °C
 30 %
@Temperature 500 °C
 40 %
@Temperature 600.0 °C
 60 %
@Temperature 700.0 °C
Machinability 65 %100% would be best rating for pre-hardened mold steels
Charpy Impact, Notched 25.0 J/cm²
@Temperature 400 °C
 29.0 J/cm²
@Temperature 500 °C
 29.0 J/cm²
@Temperature 300 °C
 29.0 J/cm²
@Temperature 23.0 °C
 39.0 J/cm²
@Temperature 600.0 °C
 40.0 J/cm²
@Temperature 100 °C
 45.0 J/cm²
@Temperature 200 °C
 49.0 J/cm²
@Temperature 700.0 °C
Abrasion 3.76mm2kgfx10-7, Speed = 0.656 ft/sec, Final Load = 1.5 lbs; Ohgoshi
 4.61mm2kgfx10-7, Speed = 7.8064 ft/sec, Final Load = 1.5 lbs; Ohgoshi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.94 µin/in-°F
@Temperature 20.0 - 100 °C
 6.00 µin/in-°F
@Temperature 20.0 - 200 °C
 6.61 µin/in-°F
@Temperature 20.0 - 300 °C
 7.00 µin/in-°F
@Temperature 20.0 - 400 °C
 7.28 µin/in-°F
@Temperature 20.0 - 500 °C
 7.61 µin/in-°F
@Temperature 20.0 - 600.0 °C
 7.72 µin/in-°F
@Temperature 20.0 - 700.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.32 - 0.42 %
Chromium, Cr 4.5 - 5.5 %
Iron, Fe 88.38 - 90.78 %
Manganese, Mn 1.5 %
Molybdenum, Mo 1.0 - 1.5 %
Silicon, Si 1.5 %
Vanadium, V 0.40 - 1.2 %
 
Descriptive Properties
Erosion Resistance15.2%after soaking in an aluminum bath at 1292°F for 30 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm SUPERIOR® H13 Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
304 Stainless Steel
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
International Mold Steel Premium H13 Hot Work Die and Mold Steel

NIMS05 / 17384

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.