MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schunk FH82Y5 Carbon Graphite
Categories: Carbon; Graphite

Material Notes: Typical Application Fields: Sliding rings and bearings subjected to high loads, even at elevated temperatures and in chemically aggressive media.

Information provided by Schunk Graphite Technology, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 805/62.5
Modulus of Elasticity 24.0 GPa
Flexural Strength 70.0 MPa
Compressive Strength 250 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.40 µm/m-°C
@Temperature 20.0 - 200 °C
 4.80 µm/m-°C
@Temperature 200 - 600 °C
Thermal Conductivity 10.0 W/m-K
 
Descriptive Properties
Inert Atmosphere1200°C
Oxidizing Atmosphere350°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schunk FH42Y3 Carbon Graphite
Schunk FH82Z(H)2 Carbon Graphite Resin Impregnated
Graphite, Carbon, C
NeoGraf eGRAF® HITHERM™ HT-705 Graphite
Pyrolytic Graphite, Low Temperature Isotropic (LTI)

CSCHU006 / 194763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.