MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™ HFFR 361-0190 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - UL 94 HB compliant

Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP).

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccASTM D792
Viscosity 105000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
105000 cP
@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 929210 sec; ASTM D2240
Tensile Strength at Break 12.2 MPa
@Temperature 23.0 °C
1770 psi
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 220 %
@Temperature 23.0 °C
220 %
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 57.2 kN/m326 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 193 °C360 - 379 °F
Middle Barrel Temperature 210 - 227 °C410 - 441 °F
Front Barrel Temperature 227 - 238 °C441 - 460 °F
Nozzle Temperature 227 - 238 °C441 - 460 °F
Drying Temperature 70.0 °C158 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
 
Descriptive Properties
Agency RatingsUL 94 .QMFZ2.E76261
AppearanceBlack
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Injection RateSlow-Moderate
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConnectors
 Plugs
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE)
Avient OnFlex™ V 3050D-S0097 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE)

PH0POL1237 / 145806

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.