Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Superb gloss and transparency
- Exceptional printability
- Excellent hot melt anchorage
- High consistency and stability of surface properties
- Excellent machine performance
- Excellent stiffness
- High resistance to elongation on labeling machine
- Good mold resistance
- Not humidity resistant
Features:Applications: - Beverage, Alcoholic
- Beverage, Carbonated
- Beverage, Mineral Waters
- Dairy Products
- Health and Beauty Care
Uses: Processing Method: Inner Web Adhesion Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic PrintingInformation provided by ExxonMobil |