Hostalen CRP 100 RESIST CR orange is a high density polyethylene (HDPE), orange colored similar RAL 1033 with high melt viscosity for extrusion, injection and compression molding. The compound fulfills the material requirements of EN 1555-1 and ISO 4437-1. The product is additionally classified as PE 100-RC and provides a very good long term hydrostatic strength. Especially developed for non-conventional pipe installations methods the product has a superior resistance to slow crack growth. It fulfills the material requirements of PAS 1075:2009-04. Designation according ISO 1872-1: PE,EACHL,50-T003. Applications: Gas PipeInformation provided by LyondellBasell. |