MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Appeel™ 93D894 PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: Appeel™ 93D894 is a modified polyester copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide seals over a broad temperature range when sealed to APET and PETG container materials. Appeel™ 93D894 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefin or polyester resins.
Uses:
  • Lidding Sealant
Features:
  • Appeel™ 93D894 has a lower melting point than many other polyester resins, thus it is suitable for coextrusion with temperature sensitive materials.
Key attributes:
  • moderate oxygen barrier properties
  • heat sealable
  • Does not scalp most common flavorings

Characteristics/Benefits:
  • Moisture level when packed: 0.2%
  • Intrinsic Viscosity (dL/g): 0.82 +/- 0.03
Applications: Lidding and Pouches for Packaging

Availability: Africa & Middle East; Asia Pacific; Latin America; Europe; North America

Agency Ratings: FDA 21 CFR 176.170 ©, Table 1; FDA 21 CFR 176.170 ©, Table 2

Form: Pellets

Processing Method: Coextrusion; Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.750 - 0.950 g/cc0.0271 - 0.0343 lb/in³Apparent
Density 1.33 g/cc0.0480 lb/in³ASTM D1505
Viscosity Number 0.80 cm³/g0.0080 dl/gIntrinsic; ASTM D5225
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FASTM D3418
Glass Transition Temp, Tg 76.1 °C169 °FASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF406 / 311099

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.