MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lion SBR 1012 Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Hot polymerized SBR 1012 elastomer is particularly useful as a binder for fibrous materials. It imparts increased cohesive strength when added to an adhesive mixture.

Unique Features:

  • Hot polymerized styrene-butadiene elastomer
  • Broad molecular weight makes dissolving easier
  • High Mooney and higher solution viscosity
Applications:
  • Binder for fibrous materials
  • Pressure sensitive and tape adhesives
  • General purpose adhesives

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D-792
Volatiles <= 1.0 %ZS 1008K
Viscosity <= 500 cPaged, 4% Toluene solution
Mooney Viscosity 105 - 135
@Temperature 100 °C
ML 1+4
Ash <= 1.5 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22.5 - 24.5 %Bound
 
Descriptive Properties
ColorOff White
Content<0.5%Soap
 4-6%Organic acid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLION072 / 317981

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.