MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eagle Brass 18665 MSP1, Annealed
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs, switches, sockets, and junction boxes.

Information provided by Eagle Brass Company

Key Words: UNS C18665
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³Annealed
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate <= 393 MPa<= 57000 psi
Elongation at Break >= 25 %>= 25 %in 2 in.
Tensile Modulus 117 GPa17000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000283 ohm-cm0.00000283 ohm-cmAnnealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.3 µm/m-°C
@Temperature 20.0 - 300 °C
9.60 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 456.5 W/m-K3168 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99 %99 %
Magnesium, Mg 0.70 %0.70 %
Phosphorus, P 0.040 %0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C19700, H02 Temper
Copper, UNS C65400, H01 Temper strip
Copper-Nickel-Phosphorus alloy, UNS C19000
Overview of materials for Copper Alloy
Eagle Brass 101 OFE COPPER (Certified), Hard

NEAGLE033 / 147282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.