MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik ACEMATT® OK 500 Silica
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Properties and applications: ACEMATT OK 500 is a fine-grained wax after-treated precipitated silica, which is suitable for pigmented as well as non-pigmented systems and due to the excellent suspension behavior particularly applicable in clear coatings. Films with superior surface smoothness are obtained. The physical properties of ACEMATT OK 500 make it an all-purpose matting agent. In cases where extended drying times are observed using ACEMATT OK 412, we would recommend ACEMATT OK 500 as a substitute.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 6.3 µmd50; ISO 13320-1
pH 6.35% in water; ISO 787-9
Specific Surface Area 130 m²/gISO 9277
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 5.5 %ISO 3262-19
SiO2 >= 98 %ISO 3262-19
 
Descriptive Properties
Content<1%Sulfate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIM026 / 197230

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.