MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® STAT A 40 FC BK PA66-CF40
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Carbon Fiber Filled

Material Notes: Vydyne STAT A 40 FC BK is standard flow 40% carbon-fiber reinforced PA66 resin. Available in black, it is specifically designed for high stiffness and strength. This product is also electrically conductive.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccDAM; ISO 1183
Moisture Absorption at Equilibrium 1.6 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 215 MPa50% RH; ISO 527-2
 260 MPaDAM; ISO 527-2
Elongation at Break 1.5 %DAM; ISO 527-2
 2.5 %50% RH; ISO 527-2
Tensile Modulus 18000 MPa50% RH; ISO 527-2
 25000 MPaDAM; ISO 527-2
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 15.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 255 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °CUnannealed; DAM; ISO 75-2/A
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 270 - 280 °CInjection
Middle Barrel Temperature 270 - 295 °CInjection
Front Barrel Temperature 270 - 295 °CInjection
Nozzle Temperature 270 - 295 °CInjection
Melt Temperature 270 - 295 °CInjection
Mold Temperature 70.0 - 90.0 °CInjection
Drying Temperature 90.0 - 110 °CInjection
Dry Time >= 3.00 hourInjection
 
Descriptive Properties
AdditiveLubricant
AppearanceBlack
FeaturesChemical Resistant
 Gasoline Resistant
 General Purpose
 Good Dimensional Stability
 Good Flow
 Good Stiffness
 High Tensile Strength
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9366 / 287657

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.