MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Danquinsa DANCOLL® 400 PU dispersion
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DANCOLL 400 is an aqueous, anionic, strong crystallizing PU dispersion for the one and two component application. This dispersion acts as raw material for environmental friendly adhesives coating masses. Adhesive films, produced with DANCOLL 400 distinguish themselves through its good reactivation properties and high thermo bond stability. Adhesive composites produced with adhesives based on DANCOL 400 are very good heat resistant.

Application: DANCOLL 400 serves as basic raw material for the production of one component and two component adhesives. Adhesives, produced with DANCOLL 400, are best suitable for:

  • Lamination of thermoplastic films by means of wood materials as for example membrane presses
  • Thermoforming and press lamination for the area of automotive
  • Lamination of textiles, wood, paper, PVC and a lot of other materials
  • Fixation of shoe soles and assembling of shoe uppers
  • Environmental friendly glues for offices and Household
For the processing at the two component process we would recommend the crosslinking based on aqueous, dispersible isocynates based on polyfunctional aziridine or carbodiimides or melamine formaldehyde.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³dispersion; DIN 51.757
 1.20 g/cc0.0434 lb/in³polymer content; DIN 51.757
Solids Content 38 - 42 %38 - 42 %DIN 53.189
Particle Size 100 - 300 µm100 - 300 µm
pH 6.0 - 9.06.0 - 9.0DIN 53.785
Brookfield Viscosity 400 - 800 cP400 - 800 cPRVT
Storage Temperature >= 4.00 °C>= 39.2 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 88 - 9388 - 93Micro-hardness; DIN 53.505
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 240 °C428 - 464 °Fnot cross linked
 >= 260 °C>= 500 °Fcross linked, KOFLER
Softening Point 70.0 - 80.0 °C158 - 176 °FKOFLER
Glass Transition Temp, Tg -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspectmilky and white liquid
Minimum film formation temperature5.0 °CDIN 53.787
TypePolyester polyurethane dispersion, anionic, aliphatic
UV-resistancevery good, lightfast ness 7DIN 54.004

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ034 / 294454

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.