MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASINT 4011 Polyimide, Yellow (PI)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.

Main features: Very high thermal and oxidative resistance, high creep resistant, good radiation-resistance, high toughness, very good chemical resistance, very low absorption of water, low outgassing, good electrical insulating, easily machined, sensitive to hydrolysis in higher thermal range, flame retardant according to UL94 V-0

Applications: Mechanical engineering, precision engineering, semiconductor, electronics, conveyor technology, electrical engineering

Preferred Fields: Valve seating, seals, insulators, lead backer, carriage, test sockets

Information Provided by Ensinger Sintimid

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.416 g/cc0.05116 lb/in³DIN 53 479
Water Absorption  0.16 %
@Temperature 23.0 °C
0.16 %
@Temperature 73.4 °F
24 hours in water; EN ISO 62
 0.60 %
@Temperature 80.0 °C
0.60 %
@Temperature 176 °F
24 hours in water; EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 88
@Temperature 23.0 °C
88
@Temperature 73.4 °F
DIN 53 505
Tensile Strength 124 MPa
@Temperature 23.0 °C
18000 psi
@Temperature 73.4 °F
EN ISO 527
Elongation at Break 4.5 %
@Temperature 23.0 °C
4.5 %
@Temperature 73.4 °F
EN ISO 527
Tensile Modulus 3.90 GPa
@Temperature 23.0 °C
566 ksi
@Temperature 73.4 °F
EN ISO 527
Flexural Strength 197 MPa
@Temperature 23.0 °C
28600 psi
@Temperature 73.4 °F
EN ISO 178
Flexural Modulus 4.316 GPa
@Temperature 23.0 °C
626.0 ksi
@Temperature 73.4 °F
EN ISO 178
Flexural Strain at Yield 7.5 %
@Temperature 23.0 °C
7.5 %
@Temperature 73.4 °F
EN ISO 178
Compressive Yield Strength 185 MPa
@Strain 10 %,
Temperature 23.0 °C
26800 psi
@Strain 10 %,
Temperature 73.4 °F
EN ISO 604
Compressive Strength 570 MPa
@Temperature 23.0 °C
82700 psi
@Temperature 73.4 °F
EN ISO 604
Compressive Modulus 2.36 GPa
@Temperature 23.0 °C
342 ksi
@Temperature 73.4 °F
EN ISO 604
Charpy Impact Unnotched 7.20 J/cm²
@Temperature 23.0 °C
34.3 ft-lb/in²
@Temperature 73.4 °F
EN ISO 179
Compression Set 70 %
@Temperature 23.0 °C
70 %
@Temperature 73.4 °F
Compression at Break; EN ISO 604
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm
@Temperature 23.0 °C
1.00e+16 ohm-cm
@Temperature 73.4 °F
IEC 60093
Surface Resistivity per Square 1.00e+16 ohm
@Temperature 23.0 °C
1.00e+16 ohm
@Temperature 73.4 °F
IEC 60093
Dielectric Strength 18.0 kV/mm
@Temperature 23.0 °C
457 kV/in
@Temperature 73.4 °F
ISO 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 45.0 µm/m-°C
@Temperature 50.0 - 200 °C
25.0 µin/in-°F
@Temperature 122 - 392 °F
DIN 53 752
CTE, linear, Transverse to Flow 57.0 µm/m-°C
@Temperature 50.0 - 200 °C
31.7 µin/in-°F
@Temperature 122 - 392 °F
DIN 53 752
Specific Heat Capacity 1.04 J/g-°C0.249 BTU/lb-°F
Thermal Conductivity 0.400 W/m-K
@Temperature 40.0 °C
2.78 BTU-in/hr-ft²-°F
@Temperature 104 °F
ISO 8302
Glass Transition Temp, Tg 260 °C500 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger TECASINT 5011 Polyimide (PI)
Ensinger TECASINT 1101 Polyimide (PI)
Hippe PI
Ensinger TECASINT 1041 Polyimide, 30% MoS2 Filled (PI)
Ensinger TECASINT 3032 Polyimide, Black, 40% Graphite (PI)

PENSIN080 / 121083

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.