MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sharadaa Ceramics Sharada RFC-95 Gel Bonded Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Mullite Bonded Free Flowing Cement Free Versatile Castable System

Product Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, Extreme resistance to thermal, Ultra high creep resistance-High HMOR, Intricate shaped Precast blocks superior to fired and Resistance to Mill scale /Accretion

Industry Focus: Steel: Blast Furnace Trough, Torpedo Ladles, Lances/Snorkel, Burner Blocks, Reheat furnace roof/Hearth, Coke Oven door/Roof Repair, Sponge Iron DRI Maintenance, Tundish Flow control device/Well blocks/Nozzles; Cement: Burner Pipe; Non Ferrous: Non wetting to Aluminum/Copper, Lined in Melting furnace walls, Launders, Aluminum Transfer Ladles; Ceramic: Fused silica kiln furniture for Ultra Low thermal, Expansion and High resistance to thermal shock; Ferrous Foundry: Ladles; Glass: Repair of Silica Roof, Sub paving.

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.80 g/cc
@Temperature 1400 °C
 2.90 g/cc
@Temperature 800 °C
 3.00 g/cc
@Temperature 200 °C
Porosity 12 %
 13 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.200 GPa
@Temperature 1400 °C
Hot
Compressive Strength 700 kg(f)/cm²
@Temperature 800 °C
Cold Crushing
 900 kg(f)/cm²
@Temperature 1400 °C
Cold Crushing
 
Component Elements PropertiesOriginal ValueComments
Al2O3 95 %
Fe2O3 0.30 %
 
Descriptive Properties
Base MaterialWhite Fused Alumina
Permanent Linear Change-1.0 - 1.0%1400°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Fused Silica Cast Thermal Ceramic
Pyrotek Pyrocast AR-S Castable Refractory
Pyrotek Pyrocast AR Castable Refractory
Sharadaa Ceramics Sharada RFC-Fused Silica Gel Bonded Castables

CSHARA058 / 130221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.