MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.

Data provided by High Performance Alloys, Inc. and Haynes International.

Key Words: ASME SB-333, ASME SB-335, ASME SB-619, ASME SB-622, ASME SB-626 UNS N10665
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.22 g/cc0.333 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 415415Estimated from Rockwell C
Hardness, Rockwell A 7373Estimated from Rockwell C
Hardness, Rockwell C 4545
Hardness, Vickers 440440Estimated from Rockwell C
Modulus of Elasticity  189 GPa
@Thickness 12.7 mm,
Temperature 538 °C
27400 ksi
@Thickness 0.500 in,
Temperature 1000 °F
(Heat treated at 1066°C (1950°F), rapid quenched, plate)
 196 GPa
@Thickness 12.7 mm,
Temperature 427 °C
28400 ksi
@Thickness 0.500 in,
Temperature 800 °F
(Heat treated at 1066°C (1950°F), rapid quenched, plate)
 202 GPa
@Thickness 12.7 mm,
Temperature 316 °C
29300 ksi
@Thickness 0.500 in,
Temperature 600 °F
(Heat treated at 1066°C (1950°F), rapid quenched, plate)
 217 GPa
@Thickness 12.7 mm,
Temperature 21.1 °C
31500 ksi
@Thickness 0.500 in,
Temperature 70.0 °F
(Heat treated at 1066°C (1950°F), rapid quenched, plate)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.000137 ohm-cm
@Temperature 0.000 °C
0.000137 ohm-cm
@Temperature 32.0 °F
 0.000138 ohm-cm
@Temperature 100 °C
0.000138 ohm-cm
@Temperature 212 °F
 0.000138 ohm-cm
@Temperature 200 °C
0.000138 ohm-cm
@Temperature 392 °F
 0.000139 ohm-cm
@Temperature 300 °C
0.000139 ohm-cm
@Temperature 572 °F
 0.000139 ohm-cm
@Temperature 400 °C
0.000139 ohm-cm
@Temperature 752 °F
 0.000141 ohm-cm
@Temperature 500 °C
0.000141 ohm-cm
@Temperature 932 °F
 0.000146 ohm-cm
@Temperature 600 °C
0.000146 ohm-cm
@Temperature 1110 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.3 µm/m-°C
@Temperature 20.0 - 93.0 °C
5.72 µin/in-°F
@Temperature 68.0 - 199 °F
 10.8 µm/m-°C
@Temperature 20.0 - 204 °C
6.00 µin/in-°F
@Temperature 68.0 - 399 °F
 11.2 µm/m-°C
@Temperature 20.0 - 316 °C
6.22 µin/in-°F
@Temperature 68.0 - 601 °F
 11.5 µm/m-°C
@Temperature 20.0 - 427 °C
6.39 µin/in-°F
@Temperature 68.0 - 801 °F
 11.7 µm/m-°C
@Temperature 20.0 - 538 °C
6.50 µin/in-°F
@Temperature 68.0 - 1000 °F
Specific Heat Capacity  0.373 J/g-°C
@Temperature 0.000 °C
0.0891 BTU/lb-°F
@Temperature 32.0 °F
 0.389 J/g-°C
@Temperature 100 °C
0.0930 BTU/lb-°F
@Temperature 212 °F
 0.406 J/g-°C
@Temperature 200 °C
0.0970 BTU/lb-°F
@Temperature 392 °F
 0.423 J/g-°C
@Temperature 300 °C
0.101 BTU/lb-°F
@Temperature 572 °F
 0.431 J/g-°C
@Temperature 400 °C
0.103 BTU/lb-°F
@Temperature 752 °F
 0.444 J/g-°C
@Temperature 500 °C
0.106 BTU/lb-°F
@Temperature 932 °F
 0.456 J/g-°C
@Temperature 600 °C
0.109 BTU/lb-°F
@Temperature 1110 °F
Thermal Conductivity  11.1 W/m-K
@Temperature 0.000 °C
77.0 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 12.2 W/m-K
@Temperature 100 °C
84.7 BTU-in/hr-ft²-°F
@Temperature 212 °F
 13.4 W/m-K
@Temperature 200 °C
93.0 BTU-in/hr-ft²-°F
@Temperature 392 °F
 14.6 W/m-K
@Temperature 300 °C
101 BTU-in/hr-ft²-°F
@Temperature 572 °F
 16.0 W/m-K
@Temperature 400 °C
111 BTU-in/hr-ft²-°F
@Temperature 752 °F
 17.3 W/m-K
@Temperature 500 °C
120 BTU-in/hr-ft²-°F
@Temperature 932 °F
 18.7 W/m-K
@Temperature 600 °C
130 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 %0.010 %
Chromium, Cr 1.0 %1.0 %
Cobalt, Co <= 1.0 %<= 1.0 %
Iron, Fe <= 2.0 %<= 2.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 28 %28 %
Nickel, Ni 69 %69 %
Silicon, Si <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes Hastelloy® B-2 alloy, sheet and plate, 2.5-8.9 mm thick, heat treated at 1066°C, rapid quenched
660 Stainless Steel (A286) cold drawn wire diameter of 2.84 mm, aged at 650°C (1200°F)
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm
660 Stainless Steel (A286) cold drawn wire diameter of 2.84 mm
ASTM A446 Steel, grade C

NPHB24 / 18806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.